American alloy steel

API 2Y 60

Overview

This grade is very similar to API 2H 50 in both it’s make up and it’s applications. API 2Y 60 is quenched and tempered and has a 60,000 minimum yield. It is used in offshore platforms and structures where additional strength is required to resist impact and fatigue concerns.

Specifications

Specification API 2Y
Grade 60 Q & T
Type of Steel Carbon
Requirements for Delivery A6, A20
Tensile Strength (ksi) 75
Yield Strength (min. ksi)
(Yield Point if designated YP)
t 1 in. 60-90
t 60-85
Spec. Thickness (Max. in.)
Chemical Composition (%)
Carbon (Max.) 0.16
Manganese 1.15/1.60
Phosphorus (Max.) .03
Sulfur (Max.) .010
Silicon .05/.50
Nickel (Max.) 1.0
Chromium (Max.) .25
Molybdenum (Max.) .15
Copper (Max.) .35
Other Elements *
Heat Treatment Required Q & T